G12

detalhe

Description

Construction alloy steel to chromium-nickel-molybdenum, treated. 

Main applications

  • Torsion Shafts and Sprockets
  • Parts for Metalomechanics with Suitability for Heat Treatment Hardening

Delivery status

Treated

Hardness of the supply

  • Min: -
  • Med: -
  • Max: 300 HB
  • Composition
  • Services
  • Heat Treatments
  • Download

Profiles available

Thickness Tolerance
Round On Request EN 10060

Chemical composition (%) 1

Min Med Max
C
0,26 0,34
Si
0,40
Mn
0,50 0,80
P
0,025
S
0,035
Cr
1,80 2,20
Mo
0,30 0,50
Ni
1,80 2,20

Physical properties

Density : 7,80
10ˉ⁶m/mK
20 a 100 ⁰C 20 a 200 ⁰C 20 a 300 ⁰C 20 a 400 ⁰C 20 a 500 ⁰C 20 a 600 ⁰C 20 a 700 ⁰C
12,1 12,7 13,2 13,6 14,0 14,4 ---

Thermal Conductivity W/mk
20 ⁰C 200 ⁰C 300 ⁰C 350 ⁰C 400 ⁰C 600⁰C 700 ⁰C
33,7 --- 37,8 --- --- 35,7 ---

GPa
-100 ⁰C 0 ⁰C 20 ⁰C 100 ⁰C 200 ⁰C 300 ⁰C 400 ⁰C 500 ⁰C 600 ⁰C
--- 213 212 207 199 192 184 175 164

Mechanical properties

Condition Ø Thickness Mechanical properties
Hardness Rm Rp0,2 ReH A Z RC
Hardened and tempered ≤ 16 - - - - - - -
Drawn (+C) ≤ 16 - - - - - - -
Ground (+SH) ≤ 16 - - - - - - -
N/A ≤ 16 - - - - - - -
Hardened and tempered ≤ 40 - - - - - - -
Drawn (+C) ≤ 40 - - - - - - -
Ground (+SH) ≤ 40 - - - - - - -
N/A ≤ 40 - - - - - - -
Hardened and tempered ≤ 100 - - - - - - -
Drawn (+C) ≤ 100 - - - - - - -
Ground (+SH) ≤ 100 - - - - - - -
N/A ≤ 100 - - - - - - -
Hardened and tempered ≤ 160 - - - - - - -
Drawn (+C) ≤ 160 - - - - - - -
Ground (+SH) ≤ 160 - - - - - - -
N/A ≤ 160 - - - - - - -
Hardened and tempered ≤ 250 - - - - - - -
Drawn (+C) ≤ 250 - - - - - - -
Ground (+SH) ≤ 250 - - - - - - -
N/A ≤ 250 - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -

Notes on mechanical properties

Rp0

  • Composition

    Profiles available

      • Round
      • On Request
      • EN 10060

    Chemical composition (%) 1

    Min Med Max
    C
    0,26 0,34
    Si
    0,40
    Mn
    0,50 0,80
    P
    0,025
    S
    0,035
    Cr
    1,80 2,20
    Mo
    0,30 0,50
    Ni
    1,80 2,20

    Physical properties

    Density : 7,80
    10ˉ⁶m/mK
    20 a 100 ⁰C 12,1
    20 a 200 ⁰C 12,7
    20 a 300 ⁰C 13,2
    20 a 400 ⁰C 13,6
    20 a 500 ⁰C 14,0
    20 a 600 ⁰C 14,4
    20 a 700 ⁰C ---

    Thermal Conductivity W/mk
    20 ⁰C 33,7
    200 ⁰C ---
    300 ⁰C 37,8
    350 ⁰C ---
    400 ⁰C ---
    600⁰C 35,7
    700 ⁰C ---

    GPa
    -100 ⁰C ---
    0 ⁰C 213
    20 ⁰C 212
    100 ⁰C 207
    200 ⁰C 199
    300 ⁰C 192
    400 ⁰C 184
    500 ⁰C 175
    600 ⁰C 164

    Mechanical properties

    Please refer to the table in the downloads section.

    Notes on mechanical properties

    Rp0

  • Services
  • Heat Treatments
  • Download

Advanced Search

Hardness HB

Hardness HRC

Resistance to abrasive wear

Resistance to adhesive wear

Resistance to tempering

Resistance to heat wear

Resistance to fatigue

Compressive strength

Toughness

Ductility

Corrosion resistance

Machinability

Suitability for welding

Suitability for polishing

Thermal fatigue

Suitability for nitriding

Suitability for texture

Number of cycles (Durability)

Creep resistance

Hardenability

Find products

If you do not find the configuration you are looking for, please see Advanced Search.

Advanced Search