ARK J31
Description
High-speed alloyed steel used in high-wear parts such as lathe tools and dies. It has a high resistance to wear, good toughness and dimensional stability. Its mechanical properties can be improved with hardening treatment. Nitriding will favour wear and oxidation resistance.
Main applications
Delivery status
Annealed
Hardness of the supply
Standards
Profiles available
Thickness | Tolerance | |
---|---|---|
Round | 10 - 102 mm | EN 10060 |
Square | On Request | EN 10059 |
Rectangular | On Request | EN 10058 |
Chemical composition (%) 1
C |
|
|||
---|---|---|---|---|
Si |
|
|||
Mn |
|
|||
Cr |
|
|||
Mo |
|
|||
V |
|
|||
W |
|
Physical properties
20 a 100 ⁰C | 20 a 200 ⁰C | 20 a 300 ⁰C | 20 a 400 ⁰C | 20 a 500 ⁰C | 20 a 600 ⁰C | 20 a 700 ⁰C |
---|---|---|---|---|---|---|
11,5 | 11,7 | 12,20 | 12,40 | 12,70 | 13,00 | --- |
20 ⁰C | 200 ⁰C | 300 ⁰C | 350 ⁰C | 400 ⁰C | 600⁰C | 700 ⁰C |
---|---|---|---|---|---|---|
22 | --- | --- | --- | --- | --- | --- |
-100 ⁰C | 0 ⁰C | 20 ⁰C | 100 ⁰C | 200 ⁰C | 300 ⁰C | 400 ⁰C | 500 ⁰C | 600 ⁰C |
---|---|---|---|---|---|---|---|---|
--- | --- | 219 | --- | --- | --- | --- | --- | --- |
Mechanical properties
Condition | Ø | Thickness | Mechanical properties | ||||||
Hardness | Rm | Rp0,2 | ReH | A | Z | RC | |||
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
The hardness value is part of the specification of the material.
Standards
Profiles available
Chemical composition (%) 1
C |
|
|||
---|---|---|---|---|
Si |
|
|||
Mn |
|
|||
Cr |
|
|||
Mo |
|
|||
V |
|
|||
W |
|
Physical properties
20 a 100 ⁰C | 11,5 |
---|---|
20 a 200 ⁰C | 11,7 |
20 a 300 ⁰C | 12,20 |
20 a 400 ⁰C | 12,40 |
20 a 500 ⁰C | 12,70 |
20 a 600 ⁰C | 13,00 |
20 a 700 ⁰C | --- |
20 ⁰C | 22 |
---|---|
200 ⁰C | --- |
300 ⁰C | --- |
350 ⁰C | --- |
400 ⁰C | --- |
600⁰C | --- |
700 ⁰C | --- |
-100 ⁰C | --- |
---|---|
0 ⁰C | --- |
20 ⁰C | 219 |
100 ⁰C | --- |
200 ⁰C | --- |
300 ⁰C | --- |
400 ⁰C | --- |
500 ⁰C | --- |
600 ⁰C | --- |
Mechanical properties
Please refer to the table in the downloads section.
The hardness value is part of the specification of the material.