BR 3

detalhe

Description

Hard bronze with excellent mechanical strength and toughness. Excellent corrosion resistance especially in saline environments.

Main applications

  • Helical Gear
  • Nuts
  • Axis Elements subject to cavitation

Delivery status

Bled

Hardness of the supply

  • Min: 90 HB
  • Med: -
  • Max: -
  • Composition
  • Services
  • Heat Treatments
  • Download

Profiles available

Thickness Tolerance
Round 13 - 131 mm
Tube 21 - 141 mm

Chemical composition (%) 1

Min Med Max
P
0,600
Ni
2,00
Cu
85,00 89,00
Sn
10,50 13,00
Pb
0,70

Physical properties

Density : 8,90
10ˉ⁶m/mK
20 a 100 ⁰C 20 a 200 ⁰C 20 a 300 ⁰C 20 a 400 ⁰C 20 a 500 ⁰C 20 a 600 ⁰C 20 a 700 ⁰C
17,4 --- --- --- --- --- ---

Thermal Conductivity W/mk
20 ⁰C 200 ⁰C 300 ⁰C 350 ⁰C 400 ⁰C 600⁰C 700 ⁰C
50 --- --- --- --- --- ---

GPa
-100 ⁰C 0 ⁰C 20 ⁰C 100 ⁰C 200 ⁰C 300 ⁰C 400 ⁰C 500 ⁰C 600 ⁰C
--- --- 100 --- --- --- --- --- ---

Mechanical properties

Condition Ø Thickness Mechanical properties
Hardness Rm Rp0,2 ReH A Z RC
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
  • Composition

    Profiles available

      • Round
      • 13 - 131 mm
      • Tube
      • 21 - 141 mm

    Chemical composition (%) 1

    Min Med Max
    P
    0,600
    Ni
    2,00
    Cu
    85,00 89,00
    Sn
    10,50 13,00
    Pb
    0,70

    Physical properties

    Density : 8,90
    10ˉ⁶m/mK
    20 a 100 ⁰C 17,4
    20 a 200 ⁰C ---
    20 a 300 ⁰C ---
    20 a 400 ⁰C ---
    20 a 500 ⁰C ---
    20 a 600 ⁰C ---
    20 a 700 ⁰C ---

    Thermal Conductivity W/mk
    20 ⁰C 50
    200 ⁰C ---
    300 ⁰C ---
    350 ⁰C ---
    400 ⁰C ---
    600⁰C ---
    700 ⁰C ---

    GPa
    -100 ⁰C ---
    0 ⁰C ---
    20 ⁰C 100
    100 ⁰C ---
    200 ⁰C ---
    300 ⁰C ---
    400 ⁰C ---
    500 ⁰C ---
    600 ⁰C ---

    Mechanical properties

    Please refer to the table in the downloads section.

  • Services
  • Heat Treatments
  • Download

Advanced Search

Hardness HB

Hardness HRC

Resistance to abrasive wear

Resistance to adhesive wear

Resistance to tempering

Resistance to heat wear

Resistance to fatigue

Compressive strength

Toughness

Ductility

Corrosion resistance

Machinability

Suitability for welding

Suitability for polishing

Thermal fatigue

Suitability for nitriding

Suitability for texture

Number of cycles (Durability)

Creep resistance

Hardenability

Find products

If you do not find the configuration you are looking for, please see Advanced Search.

Advanced Search