RMC 16
Main applications
Delivery status
Natural
Hardness of the supply
Standards
Profiles available
Thickness | Tolerance | |
---|---|---|
Round | 16 - 280 mm | EN 10060 |
Chemical composition (%) 1
C |
|
|||
---|---|---|---|---|
Si |
|
|||
Mn |
|
|||
P |
|
|||
S |
|
|||
Cr |
|
Physical properties
20 a 100 ⁰C | 20 a 200 ⁰C | 20 a 300 ⁰C | 20 a 400 ⁰C | 20 a 500 ⁰C | 20 a 600 ⁰C | 20 a 700 ⁰C |
---|---|---|---|---|---|---|
11,1 | 12,1 | --- | 13,5 | --- | --- | --- |
20 ⁰C | 200 ⁰C | 300 ⁰C | 350 ⁰C | 400 ⁰C | 600⁰C | 700 ⁰C |
---|---|---|---|---|---|---|
41 | --- | --- | --- | --- | --- | --- |
-100 ⁰C | 0 ⁰C | 20 ⁰C | 100 ⁰C | 200 ⁰C | 300 ⁰C | 400 ⁰C | 500 ⁰C | 600 ⁰C |
---|---|---|---|---|---|---|---|---|
--- | --- | 210 | --- | --- | --- | --- | --- | --- |
Mechanical properties
Condition | Ø | Thickness | Mechanical properties | ||||||
Hardness | Rm | Rp0,2 | ReH | A | Z | RC | |||
Hardened and tempered | ≤ 16 | - | - | - | - | - | - | - | - |
Drawn (+C) | ≤ 16 | - | - | - | - | - | - | - | - |
Ground (+SH) | ≤ 16 | - | - | - | - | - | - | - | - |
N/A | ≤ 16 | - | - | - | - | - | - | - | - |
Hardened and tempered | ≤ 40 | - | - | - | - | - | - | - | - |
Drawn (+C) | ≤ 40 | - | - | - | - | - | - | - | - |
Ground (+SH) | ≤ 40 | - | - | - | - | - | - | - | - |
N/A | ≤ 40 | - | - | - | - | - | - | - | - |
Hardened and tempered | ≤ 100 | - | - | - | - | - | - | - | - |
Drawn (+C) | ≤ 100 | - | - | - | - | - | - | - | - |
Ground (+SH) | ≤ 100 | - | - | - | - | - | - | - | - |
N/A | ≤ 100 | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardened and tempered | - | - | - | - | - | - | - | - | - |
Drawn (+C) | - | - | - | - | - | - | - | - | - |
Ground (+SH) | - | - | - | - | - | - | - | - | - |
N/A | - | - | - | - | - | - | - | - | - |
Hardness in the Annealed condition. Values Rm (Kg/mm2), Rp0,2 (Kg/mm2) and A % (Lo=5Do) are core values of the core after Heat Treatment (red. 30 mm)
Standards
Profiles available
Chemical composition (%) 1
C |
|
|||
---|---|---|---|---|
Si |
|
|||
Mn |
|
|||
P |
|
|||
S |
|
|||
Cr |
|
Physical properties
20 a 100 ⁰C | 11,1 |
---|---|
20 a 200 ⁰C | 12,1 |
20 a 300 ⁰C | --- |
20 a 400 ⁰C | 13,5 |
20 a 500 ⁰C | --- |
20 a 600 ⁰C | --- |
20 a 700 ⁰C | --- |
20 ⁰C | 41 |
---|---|
200 ⁰C | --- |
300 ⁰C | --- |
350 ⁰C | --- |
400 ⁰C | --- |
600⁰C | --- |
700 ⁰C | --- |
-100 ⁰C | --- |
---|---|
0 ⁰C | --- |
20 ⁰C | 210 |
100 ⁰C | --- |
200 ⁰C | --- |
300 ⁰C | --- |
400 ⁰C | --- |
500 ⁰C | --- |
600 ⁰C | --- |
Mechanical properties
Please refer to the table in the downloads section.
Hardness in the Annealed condition. Values Rm (Kg/mm2), Rp0,2 (Kg/mm2) and A % (Lo=5Do) are core values of the core after Heat Treatment (red. 30 mm)